D 667钴基焊丝
category |
trade- |
e to china standard |
characteristics & application |
e to aws |
||||
hard-surfacing 硬 面 堆 焊 |
d 667 |
edzcr-b-15 |
hrc≥48. resistance to wear, gas corrosion and oxidation. hardfacing of blast furnace hopper and cracker part. |
|
||||
d 802 |
edcocr-a-03 |
hrc38-47. resistance to heat, wear and corrosion. hardfacing of high temperature part such as the edge of thermo-cutter. |
ecocr-a |
|||||
d 812 |
edcocr-b-03 |
hrc45-50. resistance to heat, wear and corrosion. hardfacing of high temperature part such as internal-combustion engine valve. |
ecocr-b |
|||||
d 822 |
|
hrc≥53. resistance to wear and heat, bad shock resistance. hardfacing of rotating blade wheel of boiler. |
|
|||||
d 832 |
edcocr-c-03 |
hrc≥50. wear and heat resistance. hardfacing of high temperature part such as hot-rolling guided way. |
ecocr-c |
|||||
d 842 |
edcocr-d-03 |
hrc28-38. corrosion and thermo-fatigue resistance, work harding. hardfacing of hot forging die. |
|
|||||
category 类 别 |
trade 牌 号 |
chemical composition 主要成份(%) |
characteristics & application 特性和用途 |
e to aws 相当aws |
||||
hardfacing 硬 面 堆 焊 |
s 101 |
c3 cr28 ni4 |
hrc48-54. resistance to wear, gas corrosion and oxidation. hardfacing of bucket tooth and case pump. |
|
||||
s 111 |
c1 cr29 w5 |
hrc38-47. resistance to wear and corrosion at high-temperature. hardfacing of high temperature and pressure valve. |
ecocr-a |
|||||
s 112 |
c1.5 cr29 w8 |
hrc45-50. resistance to wear and corrosion at high-temperature. hardfacing of valve and hot-rolling pass. |
ecocr-b |
|||||
s 113 |
c2.5 cr30 w17 |
hrc≥55. wear and heat resistance at high temperature, bad shock resistance. hardfacing of screw charging carriage. |
|
|||||
s 114 |
c2.5 cr30 w12 |
hrc≥53. wear and heat resistance at high temperature, bad shock resistance. hardfacing of three-cone bit. |
ecocr-c |